General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Shore D | 23.0 °C | 67 [-] Show Supplier Material materials with Dureza Shore D of 67 [-] | ASTM D785 | ||
Impact strength, Charpy notched, ASTM | 23.0 °C | 87 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 87 J/m | ASTM D256 | ||
Resistencia a la flexión | 23.0 °C | 42 MPa Show Supplier Material materials with Resistencia a la flexión of 42 MPa | ASTM D790 | ||
Resistencia a la tracción | 23.0 °C | 27 MPa Show Supplier Material materials with Resistencia a la tracción of 27 MPa | ASTM D638 | ||
Módulo de flexión | ASTM D790 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.8 - 1 % Show Supplier Material materials with Contracción of 0.8 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Air filter housing | |
Fillers | 30% Talc |