General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.99 g/cm³ Show Supplier Material materials with Densidad of 0.99 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 68 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 68 J/m | ASTM D256 | ||
Resistencia a la flexión | 23.0 °C | 35 MPa Show Supplier Material materials with Resistencia a la flexión of 35 MPa | ASTM D790 | ||
Resistencia a la tracción | 23.0 °C | 31 MPa Show Supplier Material materials with Resistencia a la tracción of 31 MPa | ASTM D638 | ||
Módulo de flexión | ASTM D790 | ||||
Resistencia a desgarros | 24.0 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 1 - 1.5 % Show Supplier Material materials with Contracción of 1 - 1.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Flame-retardant V0, halogen-free ring, TV parts, electrical parts, holiday lights, Christmas lighting |