General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 195 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 195 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 5.1 GPa Show Supplier Material materials with Módulo de flexión of 5.1 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 89 MPa Show Supplier Material materials with Resistencia a la flexión of 89 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.2 - 0.5 % Show Supplier Material materials with Contracción of 0.2 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | High-strength, high-heat-resistant washing machine parts and mechanical parts | |
Fillers | 50% Glass Fiber |