General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.16 g/cm³ Show Supplier Material materials with Densidad of 1.16 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 117 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 117 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3.9 GPa Show Supplier Material materials with Módulo de flexión of 3.9 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la flexión of 110 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.4 - 0.8 % Show Supplier Material materials with Contracción of 0.4 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Washing machine parts | |
Fillers | 30% Glass Fiber |