General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.36 g/cm³ Show Supplier Material materials with Densidad of 1.36 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 12.8 GPa Show Supplier Material materials with Módulo de flexión of 12.8 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 282 MPa Show Supplier Material materials with Resistencia a la flexión of 282 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 186 MPa Show Supplier Material materials with Resistencia a la tracción of 186 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | New energy vehicles, smart devices, low-carbon travel equipment, mine equipment, etc. | |
Fillers | 30% Carbon Fiber |