General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Densidad of 1.17 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1 - 2 % Show Supplier Material materials with Elongación of 1 - 2 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 750 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 750 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 15.2 GPa Show Supplier Material materials with Módulo de flexión of 15.2 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 19.8 GPa Show Supplier Material materials with Módulo elástico of 19.8 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 319 MPa Show Supplier Material materials with Resistencia a la flexión of 319 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 221 MPa Show Supplier Material materials with Resistencia a la tracción of 221 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Sports equipment, lighting fixtures, power tool accessories, auto parts | |
Fillers | 30% Carbon Fiber |