General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 50 % Show Supplier Material materials with Elongación of 50 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 48 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 48 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 1.18 GPa Show Supplier Material materials with Módulo de flexión of 1.18 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 1.24 GPa Show Supplier Material materials with Módulo elástico of 1.24 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 48 MPa Show Supplier Material materials with Resistencia a la flexión of 48 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 42 MPa Show Supplier Material materials with Resistencia a la tracción of 42 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.5 - 1 % Show Supplier Material materials with Contracción of 0.5 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automobile fuel delivery pipes, automobile brake pipes, air conditioning pipes, pneumatic equipment hoses, industrial high-pressure hydraulic pipes, pipe quick connectors, automobile anti-lock brake system solenoid shafts, precision gears |