General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.1 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Charpy notched, ASTM | 23.0 °C | 600 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 600 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 1.5 GPa Show Supplier Material materials with Módulo de flexión of 1.5 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la flexión of 60 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 1.4 - 1.8 % Show Supplier Material materials with Contracción of 1.4 - 1.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Wheelchair wheels, floor expansion tubes, electrical enclosures, auto parts, rollers, sports equipment, etc. | |
Fillers | Molybdenum Disulfide |