General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.54 g/cm³ Show Supplier Material materials with Densidad of 1.54 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 110 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 110 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 11 GPa Show Supplier Material materials with Módulo de flexión of 11 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 269 MPa Show Supplier Material materials with Resistencia a la flexión of 269 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 183 MPa Show Supplier Material materials with Resistencia a la tracción of 183 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 288 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 288 °C | ASTM D648 | |
Inflamabilidad | UL94 v0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Vacuum suction pen handle, semiconductor, bushing, bearing, seal, support ring. | |
Fillers | 30% Glass Fiber |