General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.55 g/cm³ Show Supplier Material materials with Densidad of 1.55 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.2 % Show Supplier Material materials with Elongación of 2.2 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 87 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 87 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 8.2 GPa Show Supplier Material materials with Módulo de flexión of 8.2 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 117 MPa Show Supplier Material materials with Resistencia a la tracción of 117 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 215 °C | ASTM D648 | |
Inflamabilidad | UL94 V0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Wire protective shell, rim cover; OA fan, keyboard, fishing tackle reel, parts, lampshade; | |
Fillers | 20% Glass Fiber |