General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.62 g/cm³ Show Supplier Material materials with Densidad of 1.62 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 8.27 GPa Show Supplier Material materials with Módulo de flexión of 8.27 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 220 °C | ASTM D648 | |
Inflamabilidad | UL94 V0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Fuseless circuit breakers, electromagnetic switches, flyback transformers, household appliances handles, connectors, housings; Fans, keyboards, parts, lampshades. Vacuum cleaner components, electric fans, hair dryer shells, coffee utensils, etc., switches, motor shells, fuse boxes, door handles, bumpers, switchboard covers, mudguards, wire protection shells, rim covers, heat dissipation Window grilles, body panels, wheel covers, door and window parts, etc. | |
Fillers | 30% Glass Fiber |