General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 85 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 6.89 GPa Show Supplier Material materials with Módulo de flexión of 6.89 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 172 MPa Show Supplier Material materials with Resistencia a la tracción of 172 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 250 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 250 °C | ASTM D648 | |
Inflamabilidad | UL94 HB |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.4 - 0.7 % Show Supplier Material materials with Contracción of 0.4 - 0.7 % |
Technological properties
Property | ||
---|---|---|
Application areas | Cutting machine, electric saw, electric drill, angle grinder, polisher, electric hammer, electric pick, hot air gun, lithium battery screwdriver, sanding machine, engraving machine, etc.; cooling water chamber, intake manifold, mirror frame bracket, pass style Barriers, door handles, throttle bodies, fan covers, shift lever covers, hand brakes, accelerator pedals, gears, etc.; water pumps, water valves, bearings, bushings, gears, brackets, rollers, etc.; ski equipment, strollers, bicycles , Seat bracket, pulley, shaft, shredder gear, printer parts, etc. | |
Fillers | 33% Glass Fiber |