General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.58 g/cm³ Show Supplier Material materials with Densidad of 1.58 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1 % Show Supplier Material materials with Elongación of 1 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 85 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 10.7 GPa Show Supplier Material materials with Módulo de flexión of 10.7 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 107 MPa Show Supplier Material materials with Resistencia a la tracción of 107 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 260 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 260 °C | ASTM D648 | |
Inflamabilidad | UL94 V0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.35 % Show Supplier Material materials with Contracción of 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Impellers, blades, gears, eccentric wheels, bearings, clutches and wear-resistant parts; p transformer skeletons, high-frequency coil skeletons, plugs, sockets, wiring racks, contactor drums | |
Fillers | 30% Glass Fiber |