General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4 % Show Supplier Material materials with Elongación of 4 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 12.4 GPa Show Supplier Material materials with Módulo de flexión of 12.4 GPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 104 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 104 °C | ASTM D648 | |
Inflamabilidad | UL94 HB |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.15 % Show Supplier Material materials with Contracción of 0.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductors, LCDs, electronic components Applications: storage trays, pads, rollers, bushings, IC parts, guide wheels, rollers, parts of precision measuring devices, electromagnetic wave stickers for low frequency numbers. | |
Fillers | 30% Carbon Fiber |