General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.68 g/cm³ Show Supplier Material materials with Densidad of 1.68 g/cm³ | ASTM D792 |
Recycled Content | 18 % Show Supplier Material materials with Recycled Content of 18 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 80 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 14.5 GPa Show Supplier Material materials with Módulo de flexión of 14.5 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 245 MPa Show Supplier Material materials with Resistencia a la flexión of 245 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 155 MPa Show Supplier Material materials with Resistencia a la tracción of 155 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical components (e.g. electric motors, brackets, connectors), structural applications (grills). | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Color | Black | |
Fillers | 45% Glass Fiber | |
Processing methods |