General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.42 g/cm³ Show Material materials with Densidad of 1.42 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | |
Dureza Rockwell M | 23.0 °C | 88.3 [-] Show Material materials with Dureza Rockwell M of 88.3 [-] | ISO 2039-2 |
Elongación | 23.0 °C | 45 % Show Material materials with Elongación of 45 % | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 25 % Show Material materials with Elongation at yield of 25 % | ISO 527-1/-2 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Material materials with Hardness, Rockwell R of 120 [-] | ISO 2039-2 |
Límite elástico | 23.0 °C | 71 MPa Show Material materials with Límite elástico of 71 MPa | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 2.8 GPa Show Material materials with Módulo de flexión of 2.8 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 2.9 GPa Show Material materials with Módulo elástico of 2.9 GPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -6.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA |
23.0 °C | 14 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -6.0 °C | 340 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 340 kJ/m² | ISO 179/1eU |
23.0 °C | 390 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 390 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 280 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 280 kJ/m² | ISO 180/1U |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 12 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 12 kJ/m² | ISO 180/1A |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.2E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-4 1/K | ISO 11359-1/-2 | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.1E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.1E-4 1/K | ISO 11359-1/-2 | ||
Heat deflection temperature, 0.45 MPa | 159 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 159 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 91 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 91 °C | ISO 75-1/-2 | |||
Temperatura de fusión | 178 °C Show Material materials with Temperatura de fusión of 178 °C | ISO 11357-1/-3 | 18°F/min | |||
Temperatura de reblandecimiento Vicat | 174 °C Show Material materials with Temperatura de reblandecimiento Vicat of 174 °C | ISO 306 | 90°F, 2 lbf | |||
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: 27 mm/min |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 2.1 % Show Material materials with Contracción of 2.1 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 1.9 % Show Material materials with Contracción transversal of 1.9 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 2.5 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 2.5 g/10min | ISO 1133 | 190°C/2.16kg | |
Velocidad de flujo del volumen derretido | 2.1 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 2.1 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 205°C, Min. melt temperature: 200°C, Max. melt temperature: 210°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 90-110MPa, Hold pressure time: 8s/mm |