General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.59 g/cm³ Show Material materials with Densidad of 1.59 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | |
Elongación | 23.0 °C | 2.8 % Show Material materials with Elongación of 2.8 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 15 GPa Show Material materials with Módulo de flexión of 15 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 16.5 GPa Show Material materials with Módulo elástico of 16.5 GPa | ISO 527-1/-2 |
Resistencia a la tracción | 23.0 °C | 250 MPa Show Material materials with Resistencia a la tracción of 250 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -40.0 °C | 14 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | ISO 179/1eA |
23.0 °C | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 95 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 95 kJ/m² | ISO 179/1eU |
Resistencia al choque, ensayo Izod no entallado | -40.0 °C | 13.5 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 13.5 kJ/m² | ISO 180/1A |
23.0 °C | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 15 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ISO 11359-1/-2 | -40 - 23°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 5.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 5.5E-5 1/K | ISO 11359-1/-2 | -40 - 23°C | ||
Heat deflection temperature, 1.80 MPa | 236 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 236 °C | ISO 75-1/-2 | |||
Relative temperature index, electrical | 65 °C Show Material materials with Relative temperature index, electrical of 65 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical impact | 65 °C Show Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical strength | 65 °C Show Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | 120mil | |||
Temperatura de fusión | 260 °C Show Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | first heat | |||
Temperatura de transición del vidrio | 85 °C Show Material materials with Temperatura de transición del vidrio of 85 °C | ISO 11357-1/-2 | 18°F/min | |||
Inflamabilidad | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, UL recognition: yes -, Oxygen index: 27 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: 25 mm/min |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 62631-3-1 |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 6-8h, Processing Moisture Content: ≤0.1%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Min. mold temperature: 90°C, Max. mold temperature: 110°C |