Property | Value |
---|---|
Densidad | 1.35 - 1.37 g/cm³ Show Material materials with Densidad of 1.35 - 1.37 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 2.0 - 4.0 % Show Material materials with Elongación of 2.0 - 4.0 % | |
Módulo elástico | 7.0 - 13.0 GPa Show Material materials with Módulo elástico of 7.0 - 13.0 GPa | |
Resistencia a la tracción | 155.0 - 190.0 MPa Show Material materials with Resistencia a la tracción of 155.0 - 190.0 MPa | at 2-4% strain |
Resistencia al choque, ensayo Charpy entallado | 20.0 - 35.0 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 20.0 - 35.0 kJ/m² | |
Resistencia al choque, ensayo Charpy no entallado | 65 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | |
90 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² |
Aplicaciones térmicas
Property | Value |
---|---|
Calor específico | 1400.0 - 1500.0 J/(kg·K) Show Material materials with Calor específico of 1400.0 - 1500.0 J/(kg·K) |
Conductividad térmica | 0.27 - 0.33 W/(m·K) Show Material materials with Conductividad térmica of 0.27 - 0.33 W/(m·K) |
Temperatura de fusión | 260 °C Show Material materials with Temperatura de fusión of 260 °C |
Inflamabilidad | UL 94 HB |
Eléctrico
Property | Value |
---|---|
Resistividad eléctrica | 10000000000000 Ω·m Show Material materials with Resistividad eléctrica of 10000000000000 Ω·m |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic components, lightweight replacement for metals, housings | |
Fillers | 30% Long Glass Fiber | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, compression molding |