Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 12.25-40 mm - Sheet: 75x8-85x18 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 280 [-] Show Supplier Material materials with Dureza Brinell of 280 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.005 % Show Supplier Material materials with Azufre of 0.005 % | max. |
Carbono | 1.2 - 1.35 % Show Supplier Material materials with Carbono of 1.2 - 1.35 % | |
Cobre | 0.3 % Show Supplier Material materials with Cobre of 0.3 % | max. |
Cromo | 3.8 - 4.5 % Show Supplier Material materials with Cromo of 3.8 - 4.5 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 0.2 - 0.35 % Show Supplier Material materials with Manganeso of 0.2 - 0.35 % | |
Molibdeno | 0.7 - 1.0 % Show Supplier Material materials with Molibdeno of 0.7 - 1.0 % | |
Silicona | 0.15 - 0.3 % Show Supplier Material materials with Silicona of 0.15 - 0.3 % | |
Vanadio | 3.6 - 3.9 % Show Supplier Material materials with Vanadio of 3.6 - 3.9 % | |
Wolframio | 11.5 - 12.5 % Show Supplier Material materials with Wolframio of 11.5 - 12.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, industrial metrology, finishing and milling tools, cutting wheels, structural steels, reamers, turning and grooving steels for automatic work with good cooling | |
Processing history | Annealed |