Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-250 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 620.0 - 850.0 MPa Show Supplier Material materials with Resistencia a la tracción of 620.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 1.0 % Show Supplier Material materials with Azufre of 1.0 % | max. |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % | max. |
Cromo | 17.0 - 19.0 % Show Supplier Material materials with Cromo of 17.0 - 19.0 % | |
Fósforo | 0.045 % Show Supplier Material materials with Fósforo of 0.045 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Níquel | 9.0 - 12.0 % Show Supplier Material materials with Níquel of 9.0 - 12.0 % | |
Titanio | 0.5 - 0.8 % Show Supplier Material materials with Titanio of 0.5 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical engineering, Power Generation, Fittings and accessories in boiler construction, Pipelines | |
Processing history | Quenched and Tempered |