Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-320 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 12 % Show Supplier Material materials with Elongación of 12 % | min. |
Límite elástico | 500.0 MPa Show Supplier Material materials with Límite elástico of 500.0 MPa | min., RP02 |
Resistencia a la tracción | 700.0 - 850.0 MPa Show Supplier Material materials with Resistencia a la tracción of 700.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | max. |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Boro | 0.0015 % Show Supplier Material materials with Boro of 0.0015 % | |
Carbono | 0.17 - 0.23 % Show Supplier Material materials with Carbono of 0.17 - 0.23 % | max. |
Cromo | 10.0 - 11.5 % Show Supplier Material materials with Cromo of 10.0 - 11.5 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 0.4 - 0.9 % Show Supplier Material materials with Manganeso of 0.4 - 0.9 % | |
Molibdeno | 0.5 - 0.8 % Show Supplier Material materials with Molibdeno of 0.5 - 0.8 % | |
Niobio | 0.25 - 0.55 % Show Supplier Material materials with Niobio of 0.25 - 0.55 % | |
Nitrógeno | 0.05 - 0.1 % Show Supplier Material materials with Nitrógeno of 0.05 - 0.1 % | |
Níquel | 0.2 - 0.6 % Show Supplier Material materials with Níquel of 0.2 - 0.6 % | |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Vanadio | 0.1 - 0.3 % Show Supplier Material materials with Vanadio of 0.1 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant engineering, Mechanical Engineering, Power Generation, Components for high heat resistant pipelines, steam boiler and turbine construction and parts for the chemical industry and reactor technology | |
Processing history | Quenched and Tempered |