Medidas
Property | Value |
---|---|
Dimensions | 15x6-85x22 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.85 - 0.95 % Show Supplier Material materials with Carbono of 0.85 - 0.95 % | |
Cromo | 17.0 - 19.0 % Show Supplier Material materials with Cromo of 17.0 - 19.0 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.0 % Show Supplier Material materials with Manganeso of 1.0 % | max. |
Molibdeno | 0.9 - 1.3 % Show Supplier Material materials with Molibdeno of 0.9 - 1.3 % | |
Silicona | 1.00 % Show Supplier Material materials with Silicona of 1.00 % | max. |
Vanadio | 0.07 - 0.12 % Show Supplier Material materials with Vanadio of 0.07 - 0.12 % |
Technological properties
Property | ||
---|---|---|
Application areas | Apparatus engineering, shipbuilding, wear parts, perforated (Break) discs, balance pan and scale cutting, professional knives, high-quality cutting surgical instruments, rolling bearings, screw elements, spray nozzles | |
Processing history | Annealed |