Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 25-40 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | max. |
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.3 - 0.8 % Show Supplier Material materials with Manganeso of 0.3 - 0.8 % | |
Níquel | 4.75 - 5.25 % Show Supplier Material materials with Níquel of 4.75 - 5.25 % | |
Silicona | 0.35 % Show Supplier Material materials with Silicona of 0.35 % | max. |
Vanadio | 0.05 % Show Supplier Material materials with Vanadio of 0.05 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Apparatus engineering | |
Processing history | Annealed |