Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-220 mm - Sheet: 20x15-100x10 mm - Rectangular Bar: 10-40 mm |
Mecánica
Property | Value |
---|---|
Dureza Brinell | 190.0 - 247.0 [-] Show Supplier Material materials with Dureza Brinell of 190.0 - 247.0 [-] |
Resistencia a la tracción | 1.0 - 800.0 MPa Show Supplier Material materials with Resistencia a la tracción of 1.0 - 800.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.04 % Show Supplier Material materials with Azufre of 0.04 % | max. |
Carbono | 1.1 - 1.3 % Show Supplier Material materials with Carbono of 1.1 - 1.3 % | |
Fósforo | 1.0 % Show Supplier Material materials with Fósforo of 1.0 % | max. |
Manganeso | 12.0 - 13.0 % Show Supplier Material materials with Manganeso of 12.0 - 13.0 % | |
Silicona | 0.3 - 0.5 % Show Supplier Material materials with Silicona of 0.3 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Wear-resistant components for grinding machines, such as crusher jaws, excavator bolts, excavator sleeves, gripping teeth and similarly stressed parts Safety engineering, grinding technology | |
Processing history | Solution Annealed |