Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 20-48 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 850.0 - 1250.0 MPa Show Supplier Material materials with Resistencia a la tracción of 850.0 - 1250.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | max. |
Carbono | 0.3 - 0.5 % Show Supplier Material materials with Carbono of 0.3 - 0.5 % | |
Cromo | 3.0 - 5.0 % Show Supplier Material materials with Cromo of 3.0 - 5.0 % | |
Fósforo | 0.1 % Show Supplier Material materials with Fósforo of 0.1 % | max. |
Manganeso | 18.0 - 20.0 % Show Supplier Material materials with Manganeso of 18.0 - 20.0 % | |
Nitrógeno | 0.08 - 0.12 % Show Supplier Material materials with Nitrógeno of 0.08 - 0.12 % | |
Silicona | 0.80 % Show Supplier Material materials with Silicona of 0.80 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, mechanical engineering, mechanically and thermally highly stressed components in shipbuilding, mechanical and vehicle engineering and in electrical engineering | |
Processing history | Strain Hardened |