Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 42-100 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 750.0 - 950.0 MPa Show Supplier Material materials with Resistencia a la tracción of 750.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | max. |
Carbono | 0.3 - 0.5 % Show Supplier Material materials with Carbono of 0.3 - 0.5 % | |
Cromo | 3.0 - 5.0 % Show Supplier Material materials with Cromo of 3.0 - 5.0 % | |
Manganeso | 17.0 - 19.0 % Show Supplier Material materials with Manganeso of 17.0 - 19.0 % | |
Nitrógeno | 0.1 % Show Supplier Material materials with Nitrógeno of 0.1 % | max. |
Níquel | 1 % Show Supplier Material materials with Níquel of 1 % | max. |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, apparatus engineering, non-magnetisable components without special resistance to corrosion attacks | |
Processing history | Strain Hardened |