Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-270 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 250 [-] Show Supplier Material materials with Dureza Brinell of 250 [-] | max. |
Elongación | 35.0 - 40.0 % Show Supplier Material materials with Elongación of 35.0 - 40.0 % | |
Límite elástico | 280.0 MPa Show Supplier Material materials with Límite elástico of 280.0 MPa | min., RP02 |
Resistencia a la tracción | 580.0 - 800.0 MPa Show Supplier Material materials with Resistencia a la tracción of 580.0 - 800.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. |
Cromo | 16.5 - 18.5 % Show Supplier Material materials with Cromo of 16.5 - 18.5 % | |
Fósforo | 0.045 % Show Supplier Material materials with Fósforo of 0.045 % | max. |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. |
Molibdeno | 2.5 - 3.0 % Show Supplier Material materials with Molibdeno of 2.5 - 3.0 % | |
Nitrógeno | 0.15 - 0.25 % Show Supplier Material materials with Nitrógeno of 0.15 - 0.25 % | |
Níquel | 13.0 - 15.0 % Show Supplier Material materials with Níquel of 13.0 - 15.0 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Metrology, mechanical engineering, connecting parts, shipbuilding | |
Corrosion properties | Resistant to intercrystalline corrosion, pitting and stress corrosion | |
Processing history | Solution Annealed |