Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 8-230 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 35 % Show Supplier Material materials with Elongación of 35 % | min. |
Límite elástico | 365.0 MPa Show Supplier Material materials with Límite elástico of 365.0 MPa | min., RP02 |
Resistencia a la tracción | 700.0 - 950.0 MPa Show Supplier Material materials with Resistencia a la tracción of 700.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. |
Cromo | 20.0 - 21.5 % Show Supplier Material materials with Cromo of 20.0 - 21.5 % | |
Manganeso | 4.0 - 6.0 % Show Supplier Material materials with Manganeso of 4.0 - 6.0 % | |
Molibdeno | 3.0 - 3.5 % Show Supplier Material materials with Molibdeno of 3.0 - 3.5 % | |
Niobio | 0.25 % Show Supplier Material materials with Niobio of 0.25 % | max. |
Níquel | 15.0 - 17.0 % Show Supplier Material materials with Níquel of 15.0 - 17.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Metrology, mechanical engineering, connecting parts, shipbuilding | |
Corrosion properties | Resistant to intercrystalline corrosion, pitting and stress corrosion | |
Processing history | Solution Annealed |