Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-50 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | max. |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. |
Cromo | 21.5 - 24.5 % Show Supplier Material materials with Cromo of 21.5 - 24.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 4.5 - 6.5 % Show Supplier Material materials with Manganeso of 4.5 - 6.5 % | |
Molibdeno | 2.8 - 3.4 % Show Supplier Material materials with Molibdeno of 2.8 - 3.4 % | |
Niobio | 0.1 - 0.3 % Show Supplier Material materials with Niobio of 0.1 - 0.3 % | |
Nitrógeno | 0.3 - 0.5 % Show Supplier Material materials with Nitrógeno of 0.3 - 0.5 % | |
Níquel | 15.5 - 18.0 % Show Supplier Material materials with Níquel of 15.5 - 18.0 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Shipbuilding, electrical engineering, mechanical engineering | |
Corrosion properties | Resistant to intercrystalline corrosion, pitting and stress corrosion | |
Processing history | Solution Annealed |