Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6 mm -50 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 9 % Show Supplier Material materials with Elongación of 9 % | min. |
Límite elástico | 550.0 MPa Show Supplier Material materials with Límite elástico of 550.0 MPa | min., RP02 |
Resistencia a la tracción | 650.0 - 850.0 MPa Show Supplier Material materials with Resistencia a la tracción of 650.0 - 850.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.08 - 0.15 % Show Supplier Material materials with Carbono of 0.08 - 0.15 % | |
Cromo | 11.5 - 13.5 % Show Supplier Material materials with Cromo of 11.5 - 13.5 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Níquel | 0.75 % Show Supplier Material materials with Níquel of 0.75 % | max. |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Connecting parts, mechanical engineering, petrochemistry, hydraulic engineering, petroleum industry, construction parts in water and steam and mildly acting agents of the food industry as well as rifle barrels | |
Processing history | Quenched and Tempered |