Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 8-80 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 200 [-] Show Supplier Material materials with Dureza Brinell of 200 [-] | max. |
Elongación | 20 % Show Supplier Material materials with Elongación of 20 % | min. |
Límite elástico | 240.0 MPa Show Supplier Material materials with Límite elástico of 240.0 MPa | min., RP02 |
Resistencia a la tracción | 400.0 - 630.0 MPa Show Supplier Material materials with Resistencia a la tracción of 400.0 - 630.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cromo | 16.0 - 18.0 % Show Supplier Material materials with Cromo of 16.0 - 18.0 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Food technology, apparatus engineering, vehicle construction, plant engineering, parts for higher corrosion requirements with good deep-drawing and polishing properties, such as cutlery, sink linings, bumpers, wheel trims etc. | |
Processing history | Annealed |