Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-80 mm - Sheet: 40x20-40x25 mm |
Mecánica
Property | Value |
---|---|
Resistencia a la tracción | 800.0 - 950.0 MPa Show Supplier Material materials with Resistencia a la tracción of 800.0 - 950.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.12 - 0.2 % Show Supplier Material materials with Carbono of 0.12 - 0.2 % | |
Cromo | 15.0 - 18.0 % Show Supplier Material materials with Cromo of 15.0 - 18.0 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Níquel | 2.0 - 3.0 % Show Supplier Material materials with Níquel of 2.0 - 3.0 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Chemical industry, Nuclear plants | |
Processing history | Quenched and Tempered |