Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-127 mm - Sheet: 50x40-70x40 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.1 % Show Supplier Material materials with Aluminio of 0.1 % | max. |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % | max. |
Cobalto | 9.3 % Show Supplier Material materials with Cobalto of 9.3 % | max. |
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % | max. |
Molibdeno | 5.0 % Show Supplier Material materials with Molibdeno of 5.0 % | max. |
Níquel | 18.5 % Show Supplier Material materials with Níquel of 18.5 % | max. |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % | max. |
Titanio | 0.75 % Show Supplier Material materials with Titanio of 0.75 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Apparatus engineering | |
Processing history | Quenched and Tempered |