Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-52.15 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Resistencia a la tracción | 770 MPa Show Supplier Material materials with Resistencia a la tracción of 770 MPa | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % | max. |
Carbono | 0.17 - 0.22 % Show Supplier Material materials with Carbono of 0.17 - 0.22 % | |
Cromo | 12.0 - 14.0 % Show Supplier Material materials with Cromo of 12.0 - 14.0 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.0 % Show Supplier Material materials with Manganeso of 1.0 % | max. |
Molibdeno | 0.9 - 1.3 % Show Supplier Material materials with Molibdeno of 0.9 - 1.3 % | |
Níquel | 1.0 % Show Supplier Material materials with Níquel of 1.0 % | max. |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant engineering, apparatus engineering, turbine blades, valve seats in superheated steam valves for temperatures up to approx. 500° C | |
Processing history | Quenched and Tempered |