Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-340 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.04 % Show Supplier Material materials with Azufre of 0.04 % | max. |
Carbono | 0.95 - 1.2 % Show Supplier Material materials with Carbono of 0.95 - 1.2 % | |
Cromo | 0.4 - 0.8 % Show Supplier Material materials with Cromo of 0.4 - 0.8 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.0 % Show Supplier Material materials with Manganeso of 1.0 % | max. |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Apparatus engineering, shipbuilding, ultra-hardenable and wear-resistant steel, especially suitable for smaller stainless steel ball bearings | |
Processing history | Annealed |