Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-325 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 15 % Show Supplier Material materials with Elongación of 15 % | min. |
Límite elástico | 650.0 MPa Show Supplier Material materials with Límite elástico of 650.0 MPa | min., RP02 |
Resistencia a la tracción | 780.0 - 980.0 MPa Show Supplier Material materials with Resistencia a la tracción of 780.0 - 980.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.05 % Show Supplier Material materials with Carbono of 0.05 % | max. |
Cromo | 12.0 - 14.0 % Show Supplier Material materials with Cromo of 12.0 - 14.0 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 0.3 - 0.7 % Show Supplier Material materials with Molibdeno of 0.3 - 0.7 % | |
Nitrógeno | 0.02 % Show Supplier Material materials with Nitrógeno of 0.02 % | max. |
Níquel | 3.5 - 4.5 % Show Supplier Material materials with Níquel of 3.5 - 4.5 % | |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Power plant construction, power generation, pumps, armatures, compressors, turbine rotors, power plant components and reactor construction | |
Processing history | Quenched and Tempered |