Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 16-165.10 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 310 [-] Show Supplier Material materials with Dureza Brinell of 310 [-] | max. |
Elongación | 20 % Show Supplier Material materials with Elongación of 20 % | min. |
Límite elástico | 550.0 MPa Show Supplier Material materials with Límite elástico of 550.0 MPa | min., RP02 |
Resistencia a la tracción | 730.0 - 930.0 MPa Show Supplier Material materials with Resistencia a la tracción of 730.0 - 930.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. |
Cromo | 24.0 - 26.0 % Show Supplier Material materials with Cromo of 24.0 - 26.0 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Molibdeno | 3.0 - 4.5 % Show Supplier Material materials with Molibdeno of 3.0 - 4.5 % | |
Nitrógeno | 0.25 - 0.35 % Show Supplier Material materials with Nitrógeno of 0.25 - 0.35 % | |
Níquel | 6.0 - 8.0 % Show Supplier Material materials with Níquel of 6.0 - 8.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, petrochemistry, apparatus engineering, chemistry, power plant construction, offshore, mechanical engineering, corrosion-resistant parts for the construction industry, mechanical engineering and general technical applications | |
Processing history | Solution Annealed |