Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-425 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 14 % Show Supplier Material materials with Elongación of 14 % | min. |
Límite elástico | 700.0 MPa Show Supplier Material materials with Límite elástico of 700.0 MPa | min., RP02 |
Resistencia a la tracción | 1.1 - 900.0 MPa Show Supplier Material materials with Resistencia a la tracción of 1.1 - 900.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.06 % Show Supplier Material materials with Carbono of 0.06 % | max. |
Cromo | 15.0 - 17.0 % Show Supplier Material materials with Cromo of 15.0 - 17.0 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 0.8 - 1.5 % Show Supplier Material materials with Molibdeno of 0.8 - 1.5 % | |
Nitrógeno | 0.02 % Show Supplier Material materials with Nitrógeno of 0.02 % | max. |
Níquel | 4.0 - 6.0 % Show Supplier Material materials with Níquel of 4.0 - 6.0 % | |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Shipbuilding, offshore, plant construction, mechanical engineering, propeller shafts, axles, pump parts, centrifuge parts | |
Processing history | Quenched and Tempered |