Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-210 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 215 [-] Show Supplier Material materials with Dureza Brinell of 215 [-] | max. |
Elongación | 30 % Show Supplier Material materials with Elongación of 30 % | min. |
Límite elástico | 170.0 MPa Show Supplier Material materials with Límite elástico of 170.0 MPa | min., RP02 |
Resistencia a la tracción | 500.0 - 700.0 MPa Show Supplier Material materials with Resistencia a la tracción of 500.0 - 700.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % | max. |
Carbono | 0.05 % Show Supplier Material materials with Carbono of 0.05 % | max. |
Cromo | 16.5 - 18.5 % Show Supplier Material materials with Cromo of 16.5 - 18.5 % | |
Fósforo | 0.045 % Show Supplier Material materials with Fósforo of 0.045 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Molibdeno | 2.5 - 3.0 % Show Supplier Material materials with Molibdeno of 2.5 - 3.0 % | |
Nitrógeno | 0.11 % Show Supplier Material materials with Nitrógeno of 0.11 % | max. |
Níquel | 10.5 - 13.0 % Show Supplier Material materials with Níquel of 10.5 - 13.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant engineering, petrochemistry, apparatus engineering, shipbuilding, chemistry, power plant construction, vehicle construction, aerospace, food technology, pharmacy, agricultural engineering | |
Processing history | Solution Annealed |