Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-70 mm - Hexagonal Bar: 13- 50 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 270 [-] Show Supplier Material materials with Dureza Brinell of 270 [-] | max. |
Elongación | 25 % Show Supplier Material materials with Elongación of 25 % | min. |
Límite elástico | 450.0 MPa Show Supplier Material materials with Límite elástico of 450.0 MPa | min., RP02 |
Resistencia a la tracción | 650.0 - 880.0 MPa Show Supplier Material materials with Resistencia a la tracción of 650.0 - 880.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. |
Cromo | 21.0 - 23.0 % Show Supplier Material materials with Cromo of 21.0 - 23.0 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Molibdeno | 2.5 - 3.01 % Show Supplier Material materials with Molibdeno of 2.5 - 3.01 % | |
Nitrógeno | 0.1 - 0.22 % Show Supplier Material materials with Nitrógeno of 0.1 - 0.22 % | max. |
Níquel | 4.5 - 6.5 % Show Supplier Material materials with Níquel of 4.5 - 6.5 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, petrochemistry, shipbuilding, apparatus engineering, chemistry, power plant construction, aerospace, offshore, power generation, rail vehicles, electrical engineering, mechanical engineering | |
Processing history | Solution Annealed and blank |