Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 12.7-165.1 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 301 [-] Show Supplier Material materials with Dureza Brinell of 301 [-] | max. |
Elongación | 25 % Show Supplier Material materials with Elongación of 25 % | min. |
Límite elástico | 550.0 MPa Show Supplier Material materials with Límite elástico of 550.0 MPa | min., RP02 |
Resistencia a la tracción | 730.0 - 930.0 MPa Show Supplier Material materials with Resistencia a la tracción of 730.0 - 930.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. |
Cobre | 1.0 - 5.0 % Show Supplier Material materials with Cobre of 1.0 - 5.0 % | |
Cromo | 24.0 - 26.0 % Show Supplier Material materials with Cromo of 24.0 - 26.0 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 1.0 % Show Supplier Material materials with Manganeso of 1.0 % | max. |
Molibdeno | 3.0 - 4.0 % Show Supplier Material materials with Molibdeno of 3.0 - 4.0 % | |
Nitrógeno | 0.2 - 0.3 % Show Supplier Material materials with Nitrógeno of 0.2 - 0.3 % | |
Níquel | 6.0 - 8.0 % Show Supplier Material materials with Níquel of 6.0 - 8.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Wolframio | 0.5 - 1.0 % Show Supplier Material materials with Wolframio of 0.5 - 1.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, petrochemistry, apparatus engineering, chemistry, power plant construction, offshore, mechanical engineering | |
Processing history | Solution Annealed |