Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-149.23 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 45 % Show Supplier Material materials with Elongación of 45 % | min. |
Límite elástico | 1150.0 MPa Show Supplier Material materials with Límite elástico of 1150.0 MPa | min., RP02 |
Resistencia a la tracción | 1220.0 - 1400.0 MPa Show Supplier Material materials with Resistencia a la tracción of 1220.0 - 1400.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.8 - 1.35 % Show Supplier Material materials with Aluminio of 0.8 - 1.35 % | |
Azufre | 0.008 % Show Supplier Material materials with Azufre of 0.008 % | max. |
Carbono | 0.05 % Show Supplier Material materials with Carbono of 0.05 % | max. |
Cromo | 12.25 - 13.25 % Show Supplier Material materials with Cromo of 12.25 - 13.25 % | |
Fósforo | 0.01 % Show Supplier Material materials with Fósforo of 0.01 % | max. |
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % | max. |
Molibdeno | 2.0 - 2.5 % Show Supplier Material materials with Molibdeno of 2.0 - 2.5 % | |
Nitrógeno | 0.01 % Show Supplier Material materials with Nitrógeno of 0.01 % | max. |
Níquel | 7.5 - 8.5 % Show Supplier Material materials with Níquel of 7.5 - 8.5 % | |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % | max. |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Vehicle construction, connecting parts, aerospace, mechanical engineering | |
Processing history | Hardened |