Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 24-150 mm - Hexagonal Bar: 17- 41 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 35 % Show Supplier Material materials with Elongación of 35 % | min. |
Límite elástico | 220.0 MPa Show Supplier Material materials with Límite elástico of 220.0 MPa | min., RP02 |
Resistencia a la tracción | 530.0 - 730.0 MPa Show Supplier Material materials with Resistencia a la tracción of 530.0 - 730.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | max. |
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % | max. |
Cobre | 1.2 - 2.0 % Show Supplier Material materials with Cobre of 1.2 - 2.0 % | |
Cromo | 19.0 - 21.0 % Show Supplier Material materials with Cromo of 19.0 - 21.0 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Molibdeno | 4.0 - 5.0 % Show Supplier Material materials with Molibdeno of 4.0 - 5.0 % | |
Níquel | 24.0 - 26.0 % Show Supplier Material materials with Níquel of 24.0 - 26.0 % | |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant engineering, petrochemistry, apparatus engineering, chemistry | |
Corrosion properties | Particularly good resistance to highly corrosive media such as phosphorus, sulphur and hydrochloric acid media | |
Processing history | Solution Annealed |