Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 6-230 mm partly ESU - Sheet: 17x15-241x63.5 - Rectangular Bar: 51 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Resistencia a la tracción | 1200 MPa Show Supplier Material materials with Resistencia a la tracción of 1200 MPa | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cobre | 3.0 - 5.0 % Show Supplier Material materials with Cobre of 3.0 - 5.0 % | |
Cromo | 15.0 - 17.0 % Show Supplier Material materials with Cromo of 15.0 - 17.0 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 0.6 % Show Supplier Material materials with Molibdeno of 0.6 % | max. |
Níquel | 3.0 - 5.0 % Show Supplier Material materials with Níquel of 3.0 - 5.0 % | |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, mechanical engineering, medical technology, aerospace, screws and spindle material in valve construction, wheel and cover discs in compressor construction | |
Processing history | Solution Annealed |