Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 10-80 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 140.0 - 215.0 [-] Show Supplier Material materials with Dureza Brinell of 140.0 - 215.0 [-] | |
Elongación | 30 % Show Supplier Material materials with Elongación of 30 % | min. |
Límite elástico | 207.0 MPa Show Supplier Material materials with Límite elástico of 207.0 MPa | min., RP02 |
Resistencia a la tracción | 500.0 - 750.0 MPa Show Supplier Material materials with Resistencia a la tracción of 500.0 - 750.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cobre | 3.0 - 5.0 % Show Supplier Material materials with Cobre of 3.0 - 5.0 % | |
Cromo | 15.0 - 17.0 % Show Supplier Material materials with Cromo of 15.0 - 17.0 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 0.6 % Show Supplier Material materials with Molibdeno of 0.6 % | max. |
Níquel | 3.0 - 5.0 % Show Supplier Material materials with Níquel of 3.0 - 5.0 % | |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Solution Annealed |