Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-230 mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cromo | 17.0 - 19.0 % Show Supplier Material materials with Cromo of 17.0 - 19.0 % | |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Níquel | 10.0 - 12.0 % Show Supplier Material materials with Níquel of 10.0 - 12.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Titanio | 0.7 % Show Supplier Material materials with Titanio of 0.7 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |