Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-240 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 331.0 - 392.0 [-] Show Supplier Material materials with Dureza Brinell of 331.0 - 392.0 [-] | |
Elongación | 8 % Show Supplier Material materials with Elongación of 8 % | min. |
Límite elástico | 1000.0 MPa Show Supplier Material materials with Límite elástico of 1000.0 MPa | min., RP02 |
Resistencia a la tracción | 1070 MPa Show Supplier Material materials with Resistencia a la tracción of 1070 MPa | min. |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cobre | 2.5 - 4.5 % Show Supplier Material materials with Cobre of 2.5 - 4.5 % | |
Cromo | 15.0 - 15.5 % Show Supplier Material materials with Cromo of 15.0 - 15.5 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 1.0 % Show Supplier Material materials with Manganeso of 1.0 % | max. |
Molibdeno | 0.5 % Show Supplier Material materials with Molibdeno of 0.5 % | max. |
Niobio | 0.005 % Show Supplier Material materials with Niobio of 0.005 % | max. |
Níquel | 3.0 - 5.5 % Show Supplier Material materials with Níquel of 3.0 - 5.5 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Hardened |