Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-240 mm - Sheet: 17x15-254x63.5 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 7 % Show Supplier Material materials with Elongación of 7 % | min. |
Límite elástico | 1000.0 MPa Show Supplier Material materials with Límite elástico of 1000.0 MPa | min., RP02 |
Resistencia a la tracción | 1070 MPa Show Supplier Material materials with Resistencia a la tracción of 1070 MPa | min. |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cobre | 0.03 % Show Supplier Material materials with Cobre of 0.03 % | max. |
Cromo | 17.0 - 19.0 % Show Supplier Material materials with Cromo of 17.0 - 19.0 % | |
Fósforo | 0.045 % Show Supplier Material materials with Fósforo of 0.045 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Niobio | 1.0 % Show Supplier Material materials with Niobio of 1.0 % | max. |
Níquel | 9.0 - 12.0 % Show Supplier Material materials with Níquel of 9.0 - 12.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Hardened |