Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 8-265 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 140.0 - 190.0 [-] Show Supplier Material materials with Dureza Brinell of 140.0 - 190.0 [-] | |
Elongación | 40 % Show Supplier Material materials with Elongación of 40 % | min. |
Límite elástico | 215.0 MPa Show Supplier Material materials with Límite elástico of 215.0 MPa | min., RP02 |
Resistencia a la tracción | 510.0 - 740.0 MPa Show Supplier Material materials with Resistencia a la tracción of 510.0 - 740.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cobre | 3.0 - 5.0 % Show Supplier Material materials with Cobre of 3.0 - 5.0 % | |
Cromo | 15.0 - 17.5 % Show Supplier Material materials with Cromo of 15.0 - 17.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 1.0 % Show Supplier Material materials with Manganeso of 1.0 % | max. |
Niobio | 0.15 - 0.45 % Show Supplier Material materials with Niobio of 0.15 - 0.45 % | |
Níquel | 3.0 - 5.0 % Show Supplier Material materials with Níquel of 3.0 - 5.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, Apparatus engineering, Power Generation, Mechanical Engineering, Power plant engineering, Nuclear, Apparatus and components for the food industry, Film Industry, Photo Industry, Household utensils | |
Processing history | Solution Annealed |