Property | Value |
---|---|
Dimensions | Round-Bar length: 100 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 192 [-] Show Supplier Material materials with Dureza Brinell of 192 [-] | max. |
Elongación | 25 % Show Supplier Material materials with Elongación of 25 % | min. |
Límite elástico | 220.0 MPa Show Supplier Material materials with Límite elástico of 220.0 MPa | min., RP02 |
Resistencia a la tracción | 420.0 - 620.0 MPa Show Supplier Material materials with Resistencia a la tracción of 420.0 - 620.0 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cromo | 17.0 - 19.0 % Show Supplier Material materials with Cromo of 17.0 - 19.0 % | |
Fósforo | 0.045 % Show Supplier Material materials with Fósforo of 0.045 % | max. |
Manganeso | 2.0 % Show Supplier Material materials with Manganeso of 2.0 % | max. |
Niobio | 1.0 % Show Supplier Material materials with Niobio of 1.0 % | max. |
Níquel | 9.0 - 12.0 % Show Supplier Material materials with Níquel of 9.0 - 12.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Plant construction, Apparatus engineering, Power Generation, Mechanical Engineering, Power plants, Plate girder and pipes in furnace construction, in apparatus engineering for air preheaters, Superheater suspensions, Annealing hoods, Rails, Barrels | |
Processing history | Annealed |